W-80 Epoxy Pigmented Coating
W-80 consists of a pigmented, high viscosity, nonylphenol-free, epoxy resin and a thickened, cycloaliphatic amine reactant.
Overview
W-80 consists of a pigmented, high viscosity, nonylphenol-free, epoxy resin and a thickened, cycloaliphatic amine reactant. This combination achieves a rheology that makes it easy to spread but also fast to return to its resting state.
Uses and Benefits
W-80 is most often used to coat vertical substrates that require a high-build, high-performance, material that will not run or sag. It can also be used as a 1-coat line striping material, pigmented grout coat on aggregate-filled mortar and coving and as a base and saturant coat for imbedding fiberglass and carbon-fiber sheeting.
Limitations
W-80 is designed to be applied between 8-20 mils depending on the porosity of substrate. Ideal application temperatures to be between 60-90°F. Cooler temperatures will increase cure times. Warmer temperatures will decrease working and cure times. Verify that substrate temperature is above 5 degrees of dewpoint during application and cure of material to avoid a potential amine blush.
Preparation
The preparation method for each project is determined by a full understanding of the substrate to be coated, the chemistry of the coating system being used, the coating system thickness, and numerous other factors. The coating installer should fully read and understand ICRI Guideline NO. 310.2R-2013 and OSHA 29 CFR 1926.1153 before starting preparatory work. The aim, of preparing a substrate for coating applications, is to roughen the surface, remove weak layers, contaminants, dirt, debris and present a solid, clean, dry substrate for the primer. If unsure as to the level of preparation needed contact Polymer Nation at Lab@polymerNation.com.
Key Benefits
- Stain Resistant
- Durable
- Easy Maintenance
- Impact Resistant
- Low Odor/VOCs
- Abrasion Resistant
- Hygienic
Technical Data
At a glance — the specs most teams decide on.
- Shore Hardness @ 24 Hours
- 65Shore D
- Shore Hardness @ 7 Days
- 75-80Shore D
- Gloss @ 60° Angle
- 85-90Applying material close to dew point will decrease gloss and may result in an amine blush
- VOCs of Mixed Material
- <50 g/lEPA Method 24
- Color Scale per ASTM D1500
- 0.5-1.0Clear to slightly amber before filler is introduced
- Solids by Volume (Mixed)
- 100%
- Working Time
- 30-45 minutes
- Gel Time
- 50 min.Warmer temperatures will decrease gel time and lower temperatures will increase gel time
- Dry to Touch
- 6-8 hoursWarmer temperatures will reduce time and colder temperatures will increase time
- Through Dry
- 8-12 hoursWarmer temperatures will reduce time and colder temperatures will increase time
- Dry to Walk
- 12 HoursWarmer temperatures will reduce time and colder temperatures will increase time
- Dry to Lightly Use
- 16-24 hoursWarmer temperatures will reduce time and colder temperatures will increase time
- Full Cure
- 7 daysWarmer temperatures will reduce time and colder temperatures will increase time
- Number of Components
- 21-2 gallon container of Part A and 1-1 gallon container of Part B
- Mix Ratio (Liquids by Volume)
- 2:1It is always preferred to mix the entire kit, whenever possible, to avoid off-ratio mixtures
- Mixed Viscosity @ 25°C/77°F
- 4800 cPWarmer temperatures will reduce viscosity and lower temperatures will increase viscosity
- Ideal Application Temperature
- 60-90°FVerify that substrate temperature is above 5 degrees of dewpoint during application and cure of material to avoid a potential amine blush
- Application Thickness
- 8-20 mils
- Coverage Per Mix
- 80 – 200 sq.ft./gal.
- Odor
- Very SubtleMeasuring odor offensiveness is difficult so experience with chemicals has been consulted here
- Storage Temperature
- 60-80 degrees FStore material between 60-90 degrees F in a protected dry location.
Colors & Packaging
Colors
Tap a color to enlarge. Swatches are a representative guide — request a physical sample for color-critical work.
Packaging
- Available sizes
- 1.5 & 3 Gallons
- Note
- Material can be supplied in larger packaging upon request and with minimum quantities
Where It's Used
Markets
Animal Care
Fire Rescue & Public Safety
Food & Beverage
Manufacturing
Stadium & Arena Flooring
Correctional Government MunicipalUsed in Systems
Mixing & Application
It is always recommended to mix the entire kit, whenever possible, to avoid off-ratio mixtures. Mix ratio is 2 parts W-80 Part A to 1 part W-80 Part B. Combine all of part A and B into a single container, large enough to accept the entire kit. Mix at 350 RPM for 2-3 minutes using an appropriate mixing blade. Make sure to scrape any unmixed material off the sides of the mix vessel. Take care not to introduce excessive air during mixing.
Disposal: Dispose of material, containers, solvents, etc., per Federal, State and local guidelines, rules and laws.